Precautions:
Lamination process:
Lamination temperature(℃) | Evacuation time(min) | Lamination time(min) |
145 | 5-6 | 10-12 |
Performance Parameters:
Performance |
Projects |
Testing Standards |
Unit |
RP-J9001 |
|
Thickness |
GB/T 6672-2001 |
mm |
0.4~0.8 |
Tensile strength (after curing) |
GB/T 13022-91 |
Mpa |
≥8 |
|
Elongation at break (after curing) |
% |
≥800 |
||
Adhesive film and glass peel strength |
ASTM D903 |
N/cm |
≥70 |
|
Peel strength of adhesive film and backing plate |
N/cm |
≥40 |
||
Thermal Performance |
Systolicity |
ASTM 1204 |
MD% |
≤4 |
TD% |
≤2 |
|||
Cross-linking degree |
ASTM D2765 |
% |
≥75% |
|
Electrical performance |
Volumetric resistivity |
GB 1410-89 |
Ω.cm |
≥1.0×1015 |
|
Light transmittance (after curing)(280nm~380nm) |
GB/T 24102008 |
% |
≤30 |
Light transmittance (after curing)(380nm~1100nm) |
GB/T 2410-2008 |
% |
≥90 |
|
|
UV aging yellowing index |
GB/T29848 |
ΔYI |
<2.0 |
Humidity and heat aging yellowing index |
GB/T29848 |
ΔYI |
<4.0 |